Great idea thanks! 😀
Great idea thanks! 😀
It’s already running 225 for PLA since it’s a hardened steel nozzle, but I tried it on 230 with the same result
That’s a good point - I remember calibrating the extrusion multiplier for 0.1mm but not for 0.2mm, never thought that larger layer sizes would need independent calibrations!
Ah really! It could be possible it’s too moist - It’s been out a month or so. I’ll have to invest in a filament dryer. Appreciate the reply
Brilliant, thanks for the insight! Hopefully orcaslicer has a multiplier for each layer height - not just per filament